Skip to main content

Altitude Cladding

Northern Fir, Larch

The + product

The low moisture content and physical characteristics of the selected wood species allow for the manufacture of these wide blades which will not change over time.

  • FEATURES
    • Unfinished
    • End groove
    • Steamed: exposure to steam at a high temperature (100% humidity at 95°C for 3 weeks)
    • Thermally modified wood: structural modification of wood by applying a very high temperature in a kiln (between 185 and 212° for 48 hours)
    • Natural wood, dried to 12%
    • Planed and brushed surface (except for 12% dry, also available planed)
  • APPLICATIONS
    • Indoors: wall, ceiling
    • Exterior: facade made entirely of larch
    • and Thermally heated fir tree (between 185 and 212° for 48 hours)